CT-C50-F6-A9
Cement screed (CT)
Fiber-reinforced screed and thick-bed mortar
Dry mortar
Compressive strength of 50 N/mm² (C50) according to DIN EN 13813
Bending tensile strength 6 N/mm² (F6) according to DIN EN 13813
Wear resistance 9 cm³/ 50 cm² (A9) according to DIN EN 13813
Hardens quickly
Advantages:
Protects against bloating
Accessible after approx. 6 hours
Can be covered with tiles and slabs early on
Can be heated up after 3 days according to aRdT
Protection against moisture and frost damage (capillary water transport is prevented)
Long processing time
High processing reliability
Constant screed quality
Consumption:
approx. 20 kg/m² per cm of screed thickness